Da> What kind of solder is used on the SMD in the K3? Leaded or Unleaded ?
> And what kind of flux was used.
It is RoHS compliant.
> And not to start a another very long thread, what would people suggest
> for flux when doing mods?
> I'll use the same solder type. But maybe water soluble flux is not such
> a good idea for manual rework?
After the board is built, water soluble is not a good idea. The joints
will tend to corrode, and I don't like the idea of putting my K3 in the
family dishwasher for a complete rinse...
I use plain old tin-lead rosin-core solder for SMT rework on my K3. I
sometimes use "no clean" flux rather than rosin core. Depends on which
spool is nearer when I do the re-work. But I carefully avoid the spool
of water-soluble flux which I use for prototype construction.
The regular solder will alloy with the solder on the board, no problem.
73,
Lyle KK7P
_______________________________________________
Elecraft mailing list
Post to:
[hidden email]
You must be a subscriber to post to the list.
Subscriber Info (Addr. Change, sub, unsub etc.):
http://mailman.qth.net/mailman/listinfo/elecraft
Help:
http://mailman.qth.net/subscribers.htmElecraft web page:
http://www.elecraft.com